Typical Test Data
T.B. Numbers refer to specific Technical Bulletins which are available on request.
TYPICAL DRY FILM THICKNESS
Unreinforced: 72 microns.
Reinforced - Reemat Standard GFM: 360 microns.
Reinforced - Reemat Lite: 320 microns.
Reinforced - Reemat Decco: 625 microns.
TENSILE ELONGATION
Initial : 50% (minimum); Aged: 20% (maximum)
Reinforced - Reemat Standard: 12.0%
Reinforced - Reemat Lite: 4.5%
Reinforced - Reemat Decco: 11.0%
CHEMICAL RESISTANCE
Standard 10% solutions of acids and alkalis, including nitric acid and caustic soda, failed to cause breakdown of the membrane. TB 482/SPT
FIRE RESISTANCE
Indicative test results to BS.476 Parts 6 & 7 give a Class "0" rating.TB 484/SPT, 485/SPT
APPROXIMATE SOLIDS CONTENT
49% by weight; 36% by volume.
Specific gravity: 1.25 (nominal).
DRYING TIME
Touch dry in approximately 45 minutes at 10ºC. / 60% R.H., through cure in 1 hour. Touch dry in approximately 30 minutes at 20ºC. / 55% R.H., through cure in 45 minutes. Touch dry in approximately 15 to 20 minutes at 30ºC. / 50% to 60% R.H. Through cure in 30 to 45 minutes. TB 481/SPT
PACK SIZES
10 litres and 25 litres.